Componets |
DF-961-1 |
DF-961-2 |
|
Al2O3 (%) |
<40 |
<40 |
|
SiO2 (%) |
>60 |
>50 |
|
Fe2O3 (%) |
>3.0 |
>3.0 |
|
Density (dry) g/cm³ |
1.8-1.9 |
1.9-2.0 |
|
Heat conduct ratio W/m.k (350 ℃) |
~0.50 |
~0.50 |
|
Construction method |
Dry tamping |
|
Service temperature |
1400 ℃ |
1600 ℃ |
Applying Spot:replace refractory bricks and Al2O3 powder.
Thickness: about 200mm.
|
|